Abstract
The effect of doping SrTiO3 into BiFeO3 on the magnetic and crystal structure has been explored using powder neutron diffraction for (1−x)BiFeO3–xSrTiO3(1−x)BiFeO3–xSrTiO3 where x=0.2, 0.3, 0.4, 0.6 and 0.8. While the data are not sensitive to the cycloidal component of the magnetic ordering, the evolution of the collinear antiferromagnetic moment of the G-type antiferromagnetic component with T and x has been explored, as have structural parameters. It is found that for x≤0.4x≤0.4 pure phase samples form in the R3c cell, and for x =0.8 a non-magnetic Pm3¯m phase is obtained. The x=0.6 sample gives a mixed phase. Through the R3c phase the magnetic structure does not change appreciably apart from the reduction of magnetic moment magnitude with the increasing T and/or x. © 2013, Elsevier Inc.
Description
Keywords
Neutron diffraction, Strontium titanates, Antiferromagnetic materials, Ferroelectric materials, Perovskite, Crystal structure
Citation
Goossens, D. J., Weekes, C. J., Avdeev, M., & Hutchison, W. D. (2013). Crystal and magnetic structure of (1-x)BiFeO3-xSrTiO3 (x=0.2, 0.3, 0.4 and 0.8). Journal of Solid State Chemistry, 207, 111-116. doi:10.1016/j.jssc.2013.09.024