The hot pressing of beryllium oxide with additives.
dc.contributor.author | Bardsley, J | en_AU |
dc.contributor.author | Wulf, G | en_AU |
dc.date.accessioned | 2007-11-22T04:15:21Z | en_AU |
dc.date.accessioned | 2010-04-30T04:32:45Z | en_AU |
dc.date.available | 2007-11-22T04:15:21Z | en_AU |
dc.date.available | 2010-04-30T04:32:45Z | en_AU |
dc.date.issued | 1968-02 | en_AU |
dc.description.abstract | The effect of variations in temperature, pressure and pressure cycle on the density vs grain size relationship was determined for hot pressed, sulphate-derived UOX beryllium oxide; the effects of selected additives on the final grain size using constant hot pressing conditions were also determined. A single-ended pressing technique, incorporating an incremental build-up in the pressing pressure, was developed to produce hot pressed specimens of near theoretical density with a uniform grain size of 25u. Smaller grain sizes were not obtained by this technique owing to the onset of discontinuous grain growth at a bulk density of 97 per cent theoretical. However, by introducing a 'dwell' or 'equilibration' time at temperature before the application of the load, a theoretically dense specimen (3.010 g/cm3) was produced with a uniform 8u grain size. Carbon was the only additive which consistently refined the grain size at all levels of addition. A hot pressed specimen of 99 per cent theoretical density and 2u grain size was obtained using a standard condition of 1500°C, 250 kg/cm2 for 25 minutes, 5 volume per cent of colloidal graphite additive. | en_AU |
dc.identifier.citation | Wulf, G., Bardsley, J. (1968). The hot pressing of beo with additives (AAEC/TM440). Lucas Heights, N.S.W.: Research Establishment, Australian Atomic Energy Commission. | en_AU |
dc.identifier.govdoc | 355 | en_AU |
dc.identifier.other | AAEC-TM-440 | en_AU |
dc.identifier.uri | http://apo.ansto.gov.au/dspace/handle/10238/235 | en_AU |
dc.language.iso | en_au | en_AU |
dc.publisher | Australian Atomic Energy Commission | en_AU |
dc.subject | Carbon | en_AU |
dc.subject | Hot pressing | en_AU |
dc.subject | Beryllium oxides | en_AU |
dc.subject | Additives | en_AU |
dc.subject | Grain size | en_AU |
dc.title | The hot pressing of beryllium oxide with additives. | en_AU |