In situ neutron-diffraction study of the Ti38V30Cr14Mn18 structure during hydrogenation

No Thumbnail Available
Date
2013-11-01
Journal Title
Journal ISSN
Volume Title
Publisher
Elsevier Science BV
Abstract
The phase transformations of the Ti38V30Cr14Mn18 alloy during hydrogenation and dehydrogenation using deuterium (D2) were investigated using in situ neutron powder diffraction (NPD) at various D2 pressures up to 2 MPa. Initially, the first hydride that formed, Ti38V30Cr14Mn18D15, had the same body centered cubic (BCC) crystal structure as the starting alloy. Upon further hydrogenation, the system displays a distinct two-phase mixture of the intermediate BCC and body-centered tetragonal (BCT) phases, that exist in a ration of 1.38:1.42, respectively. At the end of the deuterium absorption, the phase pure Ti38V30Cr14Mn18D183 material forms, with a face-centered cubic (FCC) structure. Upon dehydrogenation, all hydride phases eventually returned to the initial alloy phase without any amorphization or disproportionation. Using standard Rietveld refinement, information on the variation of the deuterium site occupancy, the lattice symmetry, and the cell volume were determined during these phase changes and are presented. © 2013, Elsevier Ltd.
Description
Keywords
Thallium, Chromium, Manganese, Hydrogen, Neutron diffraction, Phase transformations
Citation
Fei, Y., Kong, X., Wu, Z., Li, H., & Peterson, V. K. (2013). In situ neutron-diffraction study of the Ti38V30Cr14Mn18 structure during hydrogenation. Journal of Power Sources, 241, 355-358. doi:10.1016/j.jpowsour.2013.04.118
Collections